    1. Prepare the surface thoroughly.
    2. Open the crack to a U-groove at least 6 mm wide and deep.
    3. Where the crack is deep, fill the groove to half depth with a polymer cement putty of ROOFCRETE AR 576 or ROOFBOND SBR 401 with cement and fine sand at 1:1:1.
    4. Seal the groove with WONDERSEAL XL acrylic latex sealant.
    5. Paint over once cured.

    For hollow, shrinkage or wide dead cracks, treat both faces and add injection grouting for complete sealing.

    Masonry walls move with weather. A cement filler cracks again, while acrylic latex sealant stays elastic and paintable, backed by a polymer cement putty for strength.

    WONDERSEAL XLDepends on crack width and depth
    ROOFCRETE AR 576500 ml to 2 litres per 50 kg cement

    Need this for your project?